316Lvs1.4404

AISI 316L (UNS S31603) and EN 1.4404 (X2CrNiMo17-12-2) describe the same stainless family, but the limits differ: Mo 2.00–3.00% vs 2.00–2.50%, Cr 16.0–18.0% vs 16.5–18.5%. Chemistry, mechanical values, 1.4432/1.4435 and ordering notes.

Chemical composition: where they differ

316L is the low-carbon, molybdenum-bearing austenitic stainless steel defined as UNS S31603 in product standards such as ASTM A240, A276 and A182; 1.4404 (X2CrNiMo17-12-2) is its counterpart in the EN 10088 series. Both definitions describe the same metallurgical grade, but the limits differ in width. Carbon is at most 0.030% in both. ASTM 316L has 16.0–18.0% chromium, 10.0–14.0% nickel and 2.00–3.00% molybdenum, while EN 1.4404 has 16.5–18.5% chromium, 10.0–13.0% nickel and 2.00–2.50% molybdenum. Silicon is at most 0.75% in ASTM A240 and at most 1.00% in EN. Sulphur is at most 0.030% in EN 10088-3 (bar); EN 10088-2, which covers flat products, is stricter (at most 0.015%).

Chemical Composition

Element316L1.4404
C≤ 0.030≤ 0.030
Si≤ 0.75≤ 1.00
Mn≤ 2.00≤ 2.00
P≤ 0.045≤ 0.045
S≤ 0.030≤ 0.030
Cr16.0–18.016.5–18.5
Ni10.0–14.010.0–13.0
Mo2.00–3.002.00–2.50

Heat (cast) analysis, % by mass.

Basis: 316L — ASTM A240/A240M1.4404 — EN 10088-3

Mechanical properties and strength

Mechanical values depend on the product standard and form. ASTM A240 (plate) and A276 (bar) require for annealed 316L at least 170 MPa yield, at least 485 MPa tensile strength and at least 40% elongation on a 50 mm gauge length; A240 also sets a maximum hardness of 217 HB. EN 10088-3 requires for solution-annealed (+AT) 1.4404 bar up to 160 mm at least 200 MPa 0.2% proof strength, 500–700 MPa tensile strength and at least 40% elongation. So the EN lower yield limit is slightly higher, and EN also sets an upper limit for tensile strength. In practice, the same heat usually meets the mechanical requirements of both standards; in design, calculations must use the values of whichever standard is the basis.

Mechanical Properties

Property316L1.4404
Yield Strength (MPa)≥ 170≥ 200
Tensile Strength (MPa)≥ 485500–700
Elongation (%)≥ 40 (L0 = 50 mm)≥ 40
Hardness (HB)≤ 217 (A240)—

Basis: 316L — ASTM A240 / A2761.4404 — +AT · d ≤ 160 mm · EN 10088-3

—: the designation sets no value for this property, or no comparable value is given here. The binding value follows the product standard, the delivery condition and the order, and is stated on the inspection certificate (EN 10204 3.1).

Heat treatment and delivery conditions

In both definitions the delivery condition is solution annealed and rapidly cooled; this dissolves carbides and gives the best corrosion resistance. Being austenitic, the grade cannot be hardened by heat treatment; strength only increases with cold working, which can also affect corrosion behaviour. Thanks to the low carbon, the risk of sensitisation after welding (chromium carbide precipitation at grain boundaries) is low, so solution annealing after welding is not needed in most applications. In long-term service at high temperature, however, the possible formation of brittle phases such as sigma phase must be considered.

Weldability and machinability

Weldability is excellent; no preheating is needed and molybdenum-bearing 316L-type filler metal is normally used. A small amount of delta ferrite is wanted in the weld metal to prevent hot cracking, whereas pharmaceutical and high-purity applications may limit the ferrite content. In machining the grade tends to work-harden: sharp tools, a steady and adequate feed and plenty of coolant are needed. Surface finish (ground, polished or electropolished) should be stated separately in the order, especially for hygienic applications.

Typical applications

316L and 1.4404 are used in chemical and pharmaceutical plants, food and beverage processing, marine and coastal applications, water treatment, heat exchangers and pressure equipment. Stainless flanges, fittings, valves, pump shafts and fasteners are typical products. In welded pipe and tank fabrication it is the standard choice because of its low carbon.

Applications

  • Chemical and pharmaceutical plants
  • Food and beverage processing equipment
  • Marine and coastal applications
  • Heat exchangers and pressure equipment
  • Stainless flanges, fittings and valves

316L or 1.4404: which to choose and when

The choice here is not between two different grades but between two standard definitions of the same grade. If the specification is based on ASTM or ASME (for example ASME B16.5 flanges or A312 pipe), 316L is requested; European pressure-equipment projects and specifications based on EN 10088 ask for 1.4404. If higher corrosion resistance is needed, the higher-molybdenum 1.4432 or the higher-nickel, low-ferrite 1.4435 can be considered in EN; the latter is common in pharmaceutical and biotech plants. The titanium-stabilised 1.4571 (316Ti) is a separate option against intergranular corrosion after welding.

Equivalence caveats and ordering notes

316L and 1.4404 are two definitions of the same grade, but because the ranges differ, not every 316L heat automatically counts as 1.4404: a heat with 2.6% molybdenum or 16.2% chromium, for example, meets 316L but not 1.4404. The reverse also applies: a 1.4404 heat with silicon above 0.75% exceeds the 316L limit in ASTM A240. Dual-certified material meeting both standards is therefore common on the market. Write the required standards together in the order (for example ASTM A276 316L / EN 10088-3 1.4404) and check in the inspection certificate (EN 10204 3.1) that the heat analysis meets both ranges, the delivery condition and, if needed, the intergranular corrosion test result.

Grade Equivalents

System316L1.4404
AISI / UNS316L / S31603≈ 316L
EN≈ X2CrNiMo17-12-2X2CrNiMo17-12-2
DIN (W.Nr.)≈ 1.44041.4404
JIS≈ SUS316L≈ SUS316L
GB (China)≈ 022Cr17Ni12Mo2≈ 022Cr17Ni12Mo2

Standards

316L

  • ASTM A240/A240M
  • ASTM A276/A276M
  • ASTM A479/A479M
  • ASTM A182 F316L
  • ASTM A312 TP316L

1.4404

  • EN 10088-2
  • EN 10088-3
  • EN 10222-5
  • EN 10272

The values on this page are reference data compiled from the published limits of the standards named. Binding values are those on the material's inspection certificate (EN 10204 3.1), according to the standard and delivery condition stated in the order.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote