Forged Bars & Pipes Technical Catalogue
High mechanical strength forged steel bars and seamless tubes for power generation, mining, and heavy industry applications
Product Types
Select for technical details
Forged Bars & Tubes: All types (3)
A short summary of each type is below. Dimension tables, materials and technical notes are on each type's own page.
Forged round steel bars in 200-1000mm diameter range, compliant with UNE 36-514-84 standard.
- Standard:
- UNE 36-514-84, EN 10250-2, EN 10308
Forged square steel bars in 150-1000mm side dimensions, compliant with UNE 36-514-84 standard.
- Standard:
- UNE 36-514-84, EN 10250-2, EN 10308
Seamless steel tubes in a wide range from 21.3x3mm to 660x100mm, compliant with EN 10297-1 standard.
- Standard:
- EN 10297-1, EN 10210-1, ASTM A106, API 5L
Related Sectors
Useful Calculation Tools
Detailed Technical Information and Quotation
Contact our expert team for detailed technical documents, application recommendations, and custom size quotations regarding this product type.
Get a QuoteWhat is a forged bar?
A forged bar is produced by pressing or hammering steel above its recrystallization temperature (~1100–1250°C). Forging closes internal voids and casting porosity, aligns the grain flow with the part geometry, and gives higher toughness, fatigue strength and internal soundness than rolled product. It is preferred for large-diameter shafts, gear blanks and critical machine parts.
Open-die forging, reduction ratio and quality assurance
In open-die forging, the material is progressively drawn out and rotated under a press; a reduction ratio of at least 3:1 is typically specified — it breaks up the ingot structure and homogenizes mechanical properties. Forgings are then normalized or quenched and tempered. Internal soundness is verified by ultrasonic testing (EN 10228 / SEP 1921). Q&T grades such as 42CrMo4, C45 and 34CrNiMo6 are the most common forged qualities; diameters beyond rolling capacity (Ø200 mm+) can only be produced by forging.
Frequently Asked Questions
Forged bar vs rolled bar — what is the difference?+
Forging closes internal porosity and aligns grain flow, giving higher toughness and fatigue strength in the same grade. Rolling is faster and cheaper; forging is chosen for large diameters and critical parts.
Why does the reduction ratio matter?+
A ratio of at least 3:1 breaks up ingot segregation and voids, guaranteeing a homogeneous, sound core. Critical specifications state it explicitly.
Which grades are supplied as forged bar?+
Most commonly Q&T steels such as 42CrMo4, C45, 34CrNiMo6 and 36CrNiMo4, plus tool steels and large-section carbon steels.
How are forged bars tested?+
Ultrasonic testing (EN 10228/SEP 1921) verifies internal soundness; chemistry and mechanical tests are reported in the EN 10204 3.1 certificate.
Related Blog Posts
Technical articles, guides and industry analyses

Welding 42CrMo4: Preheat, Interpass and PWHT for Q&T Steels
42CrMo4 and other quenched and tempered steels can be welded, but only under conditions: preheat, low-hydrogen consumables, controlled interpass temperature and post-weld heat treatment. The rule most often missed: on a quenched and tempered part, PWHT must not exceed the tempering temperature of the material. Datasheet values, the EN 1011-2 calculation and a work-order checklist.

Ultrasonic Testing of Steel Bars and Forgings: EN 10308, EN 10228-3
Ultrasonic testing looks for voids, internal cracks and inclusion clusters inside bars and forgings. We explain when EN 10308 applies to bars, EN 10228-3 to forgings, ASTM A388 to US specifications and SEP 1921 to German drawings, what the test finds and misses, and what to put in the order.