316L (1.4404)
Low carbon austenitic stainless steel. 16-18% Cr, 10-14% Ni, 2-3% Mo. Excellent corrosion resistance. Used in chemical, food, marine and pharmaceutical industries.
42CrMo4 (1.7225)
Chrome-molybdenum alloy steel. 0.42% C, 1.0% Cr, 0.2% Mo. High fatigue strength and toughness. AISI 4140 equivalent. Used for gears, shafts, bolts and flanges.
A
A105 (ASTM A105)
Carbon steel forging standard for flanges and fittings. Used in ambient and elevated temperature applications (max 425°C). Minimum tensile strength 485 MPa.
Alloy Steel
Steel type with added elements such as chromium, molybdenum, nickel, vanadium to enhance mechanical properties. Grades like 42CrMo4, 4140, F22 are used in piping systems.
API 6A
API standard defining design, material, testing and performance requirements for wellhead and christmas tree equipment in oil and natural gas production.
As-Rolled (+AR)
Condition of hot-rolled steel that has received no further heat treatment after rolling. Its properties depend on the rolling and cooling conditions; EN 10025-2 uses the symbol +AR.
ASME B16.11
Standard for forged socket-welding and threaded fittings (elbows, tees, couplings, caps): socket-welding in Class 3000, 6000 and 9000, threaded in Class 2000, 3000 and 6000. Used in small-bore piping.
ASME B16.47
Standard specifying dimensions, tolerances and pressure-temperature ratings for large diameter steel flanges from NPS 26 through NPS 60. Available in Series A and Series B.
ASME B16.5
American standard defining dimensions, tolerances, materials and pressure-temperature ratings for pipe flanges and flanged fittings from NPS 1/2 through NPS 24.
ASME B16.9
Standard defining dimensions and tolerances for factory-made wrought butt-welding fittings (elbows, tees, reducers, caps) from NPS 1/2 through NPS 48.
B
Blind Flange
A solid flange without a bore, used to close the end of a piping system or for pressure testing. Available in all pressure classes per ASME B16.5/B16.47.
Bolt Circle Diameter (PCD)
Diameter of the circle through the centres of the bolt holes (pitch circle diameter). Together with the outside diameter and the number and size of the holes, it decides whether two flanges can be bolted together.
Branch Outlet Fitting (Weldolet)
Forged fitting welded onto a run pipe to make a branch connection without a full tee; types include butt-weld (weldolet), socket-weld (sockolet) and threaded (threadolet). Standardised in MSS SP-97.
Bright Steel
Steel bars with a smooth, bright surface and tight tolerances, produced by cold drawing, peeling or grinding. Technical delivery conditions are given in EN 10277.
Brinell Hardness Test (HBW)
A hard-metal ball (usually 10 mm) is pressed into the surface with a set force and the diameter of the impression is measured. Suited to forgings, castings and coarse-grained material; standard ISO 6506-1.
C
C45 (1.0503)
Medium carbon unalloyed structural steel. 0.45% C. AISI 1045 equivalent. Good mechanical properties, widely used for shafts, pins, gears and machine parts.
Cap
A hemispherical or elliptical fitting used to close the end of a pipe. Applied by butt welding per ASME B16.9 standard.
Carbon Steel
Steel type with carbon as the main alloying element (0.05-2.0% C), offering high strength and machinability. Common grades include A105, A350 LF2, A516 Gr.70.
Case Hardening (Carburizing)
Enriching the surface of a low-carbon steel with carbon at high temperature and then hardening it, which gives a hard, wear-resistant case on a tough core. Used for EN 10084 case-hardening steels such as 16MnCr5.
CFR (Cost and Freight)
The seller pays the sea freight to the named port of destination, but the risk passes to the buyer when the goods are on board at the port of shipment. Insurance is the buyer's responsibility.
Charpy Impact Test
Pendulum test in which a notched specimen (usually V-notch, 10 × 10 × 55 mm) is broken at a set temperature; the absorbed energy KV in joules indicates toughness. Standardised in ISO 148-1; S355J2, for example, requires 27 J at −20 °C.
CIF (Cost, Insurance and Freight)
Like CFR, but the seller also takes out cargo insurance for the buyer; under Incoterms 2020 the minimum cover is Institute Cargo Clauses (C). Risk passes once the goods are on board at the port of shipment.
Cold Drawing
Process of pulling metal through a die at room temperature to reduce diameter and improve surface finish. Used in production of precision tolerance bars and tubes.
D
DAP (Delivered at Place)
The seller bears all costs and risks of bringing the goods to the named destination, ready for unloading; import clearance, duties and taxes are paid by the buyer.
DDP (Delivered Duty Paid)
The seller's maximum obligation: the goods are delivered at the named destination, cleared for import with duties and taxes paid, ready for unloading.
Decarburization
Loss of carbon from the surface layer of steel during heating in an oxidizing atmosphere. The decarburized layer is softer and lowers fatigue strength; its depth is measured to ISO 3887.
Delivery Condition
The state in which steel is supplied, written as a suffix to the grade: +AR (as rolled), +N (normalized or normalized rolled), +QT (quenched and tempered), +A (soft annealed), +C (cold drawn), +SH (peeled). The material standard ties the mechanical properties to this condition, so it must be stated in the order.
DIN 2527
German industrial standard for blind flanges in nominal pressures PN 6 through PN 400. Defines dimensional and tolerance requirements.
DN (Nominal Diameter)
Millimeter-based nominal diameter value used in European standards to specify the size of pipes and fittings. Common values range from DN 15 to DN 1500.
E
Elbow
A curved fitting used where the pipeline needs to change direction. Produced in standard angles of 45 and 90 degrees, with short and long radius options.
Elongation After Fracture (A)
Permanent increase of the gauge length after fracture in the tensile test, as a percentage of the original gauge length; a measure of ductility. For proportional specimens the gauge length is 5.65·√S0.
EN 10204 (Inspection Documents)
European standard defining the types of inspection documents for metallic products: declarations and test reports 2.1 and 2.2 issued by the manufacturer, and inspection certificates 3.1 and 3.2 based on specific inspection.
EN 1092-1
European standard for steel flanges from PN 2.5 to PN 400. Covers flange types, dimensions, facing finishes and pressure-temperature ratings.
EXW (Ex Works)
The seller makes the goods available at its own premises; from there the buyer bears all costs and risks, including loading and export clearance. The seller's minimum obligation among the Incoterms.
F
FCA (Free Carrier)
The seller delivers the goods, cleared for export, to the carrier nominated by the buyer at the named place; risk passes on handover. Suitable for all modes of transport, including containers.
Flakes (Hydrogen Cracks)
Fine internal cracks in large forgings and bars, caused by hydrogen dissolved in the steel combined with transformation stresses. They are prevented by vacuum degassing and controlled slow cooling, and detected by ultrasonic testing.
Flange Face Finish
Surface texture of the gasket seating area. Unless the order states otherwise, ASME B16.5 requires a serrated concentric or serrated spiral finish of 3.2–6.3 µm Ra on raised-face flanges.
Flat Face (FF)
Flange facing that is flat across the whole face, with a full-face gasket. Used to mate with cast-iron or non-metallic flanges, where a raised face could crack the mating flange when the bolts are tightened.
FOB (Free on Board)
Sea and inland waterway term: the seller delivers the goods, cleared for export, on board the vessel nominated by the buyer at the named port of shipment; risk passes once the goods are on board.
Forging
Process of shaping metal through plastic deformation under pressure. Open-die and closed-die forging methods are used in flange and fitting production.
G
Grain Size
Average size of the crystal grains in steel, expressed as a grain size number to ISO 643 or ASTM E112; the higher the number, the finer the grain. Fine-grained steels have better toughness, and many standards require a fine-grain structure.
H
Hardening (Quenching)
Heating steel to the austenitizing temperature and cooling it fast enough — in water, oil, polymer or gas — to form martensite. The steel becomes hard but brittle, so it is normally tempered afterwards.
Hardness (HRC, HB, HV)
Mechanical property measuring material resistance to permanent deformation. HRC (Rockwell C), HB (Brinell) and HV (Vickers) are common scales, tested per ASTM E18/E10/E92.
Heat (Ladle) Analysis
Chemical composition determined on a sample of the liquid steel during casting; it is the analysis reported on the certificate for that heat. A product analysis taken from the finished product may deviate from it within the permissible tolerances of the material standard.
Heat Number
Unique identification of a melt (heat) of steel, stamped or marked on the product and quoted on the certificate. It links each piece back to its chemical analysis and test results, providing traceability.
Heat Treatment
Controlled heating and cooling processes to modify metal mechanical properties. Normalizing, quenching, tempering and stress relieving are common methods.
Hot Rolling
Process of shaping metal by passing it between rollers above its recrystallization temperature (>900°C for steel). The primary method for steel bar and profile production.
Hydrostatic Test
Pressure test in which a pipe, valve or assembly is filled with water and held at a pressure above its rating to prove strength and tightness. Test pressure and duration are set by the product standard or applicable code.
I
Incoterms
Trade terms published by the International Chamber of Commerce (current edition Incoterms 2020) that define who pays for transport, insurance and customs, and where the risk passes from seller to buyer. Always quoted with a named place, e.g. "CIF Hamburg".
Induction Hardening
Surface hardening in which only the outer layer is heated by an induction coil and immediately quenched. Suited to medium-carbon and quenched-and-tempered steels such as C45 or 42CrMo4; the core keeps its properties.
Inspection Certificate 3.1
Document issued by the manufacturer's authorised inspection representative, independent of the manufacturing department, stating that the products comply with the order and giving the results of specific inspection on the delivered products.
Inspection Certificate 3.2
Like 3.1, but the document is prepared and validated by both the manufacturer's authorised inspection representative and the purchaser's authorised representative or an inspector designated by official regulations.
J
Jominy End-Quench Test
Hardenability test: a 25 mm diameter specimen is austenitized, quenched with a water jet at one end only, and hardness is measured along its length. Standard ISO 642; results are specified as +H, +HH or +HL bands in EN 10083 and EN 10084.
L
Lamination
Internal separation parallel to the surface of plate or bar, caused by inclusions, shrinkage cavities or porosity that were flattened during rolling without welding up; detected by ultrasonic testing.
Lap
Surface defect in which metal is folded over and pressed onto the surface during rolling or forging without welding to it; it appears as an irregular line that can be mistaken for a crack.
Lap Joint Flange
A flange used with a stub end that rotates freely on the pipe. Preferred in systems requiring frequent disassembly and reassembly.
Liquid Penetrant Testing (PT)
Surface test in which a coloured or fluorescent liquid penetrates open surface defects and is drawn out by a developer. It also works on non-magnetic materials such as austenitic stainless steel; general method ISO 3452-1, for forgings EN 10228-2.
M
Magnetic Particle Testing (MT)
Surface test for ferromagnetic materials: the part is magnetized and fine iron particles collect at surface and near-surface cracks. For steel forgings, EN 10228-1 applies.
Material Group (ASME B16.5)
Grouping of flange materials with similar pressure-temperature ratings in ASME B16.5; for example A105 forgings belong to Group 1.1 and F316 to Group 2.2. The rating tables are given per group and class.
Mill Scale
Layer of iron oxides formed on the surface of hot-rolled or forged steel. It is removed by shot blasting, pickling or peeling before coating or machining.
Mill Test Certificate (MTC / MTR)
Common name for the inspection document that accompanies a heat of steel, listing the heat number, chemical analysis, mechanical test results and heat-treatment condition. In Europe it is usually issued as an EN 10204 3.1 certificate.
N
Nitriding
Thermochemical treatment in which nitrogen diffuses into the surface at a temperature below Ac1 and forms hard nitrides. As no quenching is needed, distortion is low; EN 10085 nitriding steels contain nitride formers such as Al, Cr, Mo or V.
Non-Metallic Inclusions
Particles of oxides, sulphides, silicates or nitrides trapped in steel during melting and casting. Their type, size and amount are rated by microscopic methods such as ISO 4967 or ASTM E45; clean steels have low inclusion ratings.
Normalizing (+N)
Heating steel above its upper transformation temperature (Ac3) and cooling it in still air. It refines the grain and gives a uniform ferrite-pearlite structure; used for forgings and to reset the structure before further heat treatment.
Normalizing Rolling (+N)
Rolling in which the final deformation is carried out in a temperature range that gives a condition equivalent to normalizing, so the properties are retained after a later normalizing treatment. EN 10025 designates it +N, like normalizing.
NPS (Nominal Pipe Size)
Inch-based nominal measurement used in American standards to specify pipe and fitting sizes. For NPS 14 and above, it represents the actual outside diameter.
P
Peeled Bar (+SH)
Bar whose hot-rolled outer layer, including scale and surface defects, has been removed by a turning-type peeling operation, giving a bright surface and a tight diameter tolerance. EN 10277 designates the condition +SH.
Positive Material Identification (PMI)
On-site verification of a material's alloy composition, usually with handheld XRF or optical emission spectrometers, to confirm that the grade matches the certificate. Common for stainless and alloy components in piping.
Pressure Class
Classification system indicating the maximum pressure-temperature combination that flanges and valves can withstand. ASME: Class 150-2500; EN: PN 2.5-400.
Q
Quench Crack
Crack formed during hardening when thermal and transformation stresses exceed the strength of the steel; sharp corners, abrupt changes of section, too severe a quench or delayed tempering increase the risk.
Quenching and Tempering (+QT)
Hardening followed by tempering at a comparatively high temperature, giving high strength together with good toughness. The standard condition of EN 10083 steels such as 42CrMo4 and C45.
R
Raised Face (RF)
Flange facing in which the gasket seating area is raised above the bolting face. In ASME B16.5 the raised face height is 1.6 mm for Class 150 and 300 and 6.4 mm for Class 400 and above.
Reducer
A conical transition piece used to connect two pipes of different diameters. Available in concentric and eccentric types. Manufactured per ASME B16.9.
Reduction of Area (Z)
Maximum decrease of the cross-sectional area at the fracture of a tensile specimen, as a percentage of the original area; a ductility measure often specified for quenched-and-tempered steels and forgings.
Ring Type Joint (RTJ)
Flange facing with a machined groove for a solid metal ring gasket (oval or octagonal, ASME B16.20); the ring deforms plastically to seal. Used at high pressure and temperature.
Rockwell Hardness Test (HRC, HRB)
Hardness is derived from the permanent depth of indentation under a major load applied after a minor preload. HRC uses a diamond cone for hardened steel, HRB a ball for softer material; standard ISO 6508-1.
S
Schedule (Pipe Wall Thickness)
Standard classification number indicating pipe wall thickness. Common values: SCH 10, 20, 40, 80, 120, 160, XXS. Higher schedule numbers indicate greater wall thickness.
Seam
Longitudinal surface defect on rolled bar or wire: a narrow, straight discontinuity, often originating from cracks or porosity in the semi-finished cast product that were elongated during rolling.
Segregation
Uneven distribution of alloying elements and impurities that develops during solidification, typically with enrichment in the centre of continuously cast billets (centre segregation). It can cause banded structures and locally different properties.
Shot Blasting
Process of cleaning scale, rust and contaminants from metal surfaces using high-velocity steel shot. Used for surface preparation before painting or coating.
Shrinkage Cavity (Pipe)
Void formed in the last part of a casting or ingot to solidify because of volume contraction. If it is not cropped off, it can appear as a central defect in the rolled product.
Slip-On Flange
A flange that slips over the pipe and is welded from both inside and outside. Provides an economical solution for low-pressure systems. Conforms to ASME B16.5.
Socket Weld Flange
A flange where the pipe is inserted into a socket and fillet welded from the outside. Used in small-diameter, high-pressure lines (NPS 1/2 - 4).
Soft Annealing (+A)
Prolonged holding just below or around Ac1 followed by slow cooling, which spheroidizes the carbides and gives the lowest hardness. It improves machinability and cold formability; designated +A.
Solution Annealing (+AT)
Heat treatment of austenitic stainless steels: heating to a high temperature to dissolve carbides, then cooling rapidly. It restores corrosion resistance and ductility; designated +AT in EN 10088 and the usual delivery condition of 304 and 316 bars.
Spectacle Blind
Plate with a solid disc and a ring joined by a web, installed between two flanges to isolate a line (blind side) or allow flow (open side). Dimensions are given in ASME B16.48.
Spiral Wound Gasket
Semi-metallic gasket made of a V-shaped metal strip wound together with a soft filler such as graphite or PTFE, usually with an outer centring ring; dimensions for ASME B16.5 flanges are given in ASME B16.20.
Stainless Steel
Steel alloy containing at least 10.5% chromium with high corrosion resistance. Available in austenitic (304, 316L), ferritic (430) and martensitic (410) types.
Stress Relieving
Heating to a temperature below Ac1, holding and cooling slowly to reduce residual stresses from welding, machining or straightening, without significantly changing the microstructure.
Stub End
Short pipe piece with a flared lap, butt-welded to the pipe and used with a lap joint flange; the flange rotates freely, which eases bolt alignment. Dimensions in ASME B16.9 (long pattern) and MSS SP-43 (short pattern).
T
Tee
A T-shaped fitting used to branch off at 90 degrees from the main pipeline. Available as equal tee and reducing tee types.
Tempering
Reheating hardened steel to a temperature below Ac1 and holding it there to reduce brittleness and residual stress. The tempering temperature sets the balance between strength/hardness and toughness.
Tensile Strength
Maximum tensile stress a material can withstand before fracture (MPa or psi). A fundamental mechanical parameter for steel grade determination, tested per ASTM A370.
Tensile Test
Test in which a machined specimen is pulled to fracture, giving the yield strength (ReH or Rp0.2), tensile strength (Rm), elongation (A) and reduction of area (Z). Metallic materials are tested to ISO 6892-1; ASTM A370 is the US counterpart for steel products.
Test Report 2.2
Document in which the manufacturer declares that the products comply with the order, with test results from non-specific inspection — results from the same production, not necessarily from the delivered lot. Type 2.1 is a declaration of compliance without test results.
Thermomechanical Rolling (+M)
Rolling in which the final deformation takes place in a temperature range that produces properties a heat treatment alone cannot achieve. Because reheating can destroy these properties, later hot forming or normalizing is generally not suitable; grades to EN 10025-4 carry the letter M (e.g. S355M).
Third-Party Inspection (TPI)
Inspection by an independent body appointed by the buyer, such as SGS, Bureau Veritas or TÜV, which witnesses tests, checks dimensions and documents and may co-sign a 3.2 certificate.
Threaded Flange
A flange with internal threads that connects to the pipe by screwing without welding. Used in low-pressure, non-fire-hazard systems.
U
Ultrasonic Testing (UT)
Volumetric non-destructive test that uses high-frequency sound waves to find internal discontinuities such as cracks, inclusions or laminations. For steel forgings it is specified in EN 10228-3 (ferritic) and EN 10228-4 (austenitic), for bars in EN 10308.
V
Vickers Hardness Test (HV)
A square-based diamond pyramid is pressed into the surface and the diagonals of the impression are measured. With test forces from very low to high it covers thin sections, case-depth profiles and welds; standard ISO 6507-1.
W
Weld Bevel
Edge preparation on the ends of pipes and butt-weld fittings for welding. Per ASME B16.25 the standard bevel for wall thicknesses up to 22 mm is 37.5° ± 2.5° with a root face of 1.6 ± 0.8 mm.
Weld Neck Flange
A flange with a long tapered hub connected to the pipe by butt welding, preferred for high-pressure and high-temperature applications. Manufactured per ASME B16.5 and B16.47 standards.
Y
Yield Strength
Stress value at which a material begins to show permanent deformation (MPa). A critical parameter used in engineering design safety factor calculations.