Steel Grade Datasheet

X2CrNiMo17-12-2/ 1.4404 / 316LLow-Carbon Molybdenum Austenitic Stainless Steel

Standard
EN 10088-2 / EN 10088-3
Delivery Conditions
+AT
Density
8.00 g/cm³
W.-Nr.
1.4404

What is 1.4404 (AISI 316L)?

X2CrNiMo17-12-2 (Werkstoff No. 1.4404, AISI 316L) is an austenitic stainless steel with 16.5–18.5% chromium, 10.0–13.0% nickel and 2.00–2.50% molybdenum, with carbon limited to ≤ 0.030%. Molybdenum raises resistance to pitting and crevice corrosion in chloride media compared with 304; the low carbon reduces the risk of intergranular corrosion after welding. Solution annealed (+AT) bar has Rp0.2 ≥ 200 MPa, Rm 500–700 MPa and elongation ≥ 40% (EN 10088-3, d ≤ 160 mm). It is used in chemical, pharmaceutical and food plants and for flanges and fittings.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C≤ 0.030
Si≤ 1.00
Mn≤ 2.00
P≤ 0.045
S≤ 0.030 (EN 10088-3) · ≤ 0.015 (EN 10088-2)
Cr16.5–18.5
Mo2.00–2.50
Ni10.0–13.0
N≤ 0.11 (EN 10088:2005)

Mechanical Properties (+AT · EN 10088-3)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 160200500–70040
160 < d ≤ 250200500–70030

Hardness: +AT (solution annealed): ≤ 215 HB (EN 10088-3). Cannot be hardened by heat treatment; it work-hardens during cold forming.

1.4404 / AISI 316L properties and use

1.4404 is the molybdenum-alloyed, low-carbon austenitic grade in EN 10088-2 and EN 10088-3. Compared with molybdenum-free 1.4301 (304) it is far more resistant in chloride-containing media; with carbon ≤ 0.030% it resists intergranular corrosion without post-weld solution annealing. It does not harden by heat treatment and work-hardens during cold forming. In hot, high-chloride environments such as seawater even 316L can reach its limits; there, higher-alloyed grades such as duplex (e.g. 1.4462) are considered. On our site, the flanges (weld neck, slip-on, blind and threaded) and pipe fittings (elbow, tee, reducer) list ASTM A182 F316/F316L among their material options. ASTM 316L and EN 1.4404 are close but not identical: ASTM A182 F316L, for example, allows Mo 2.00–3.00%, Ni 10.0–14.0% and Cr 16.0–18.0%, whereas EN 1.4404 has Mo 2.00–2.50%. Material made to ASTM therefore does not always meet the EN ranges; the order should state the governing standard and, if needed, dual certification (316/316L or 316L/1.4404). For a quotation, state the product type (e.g. flange type and pressure class, fitting type or another form), dimensions, governing standard and quantity. Aktif Çelik reviews the request through its supply network and prepares a quote; the material can be requested with an EN 10204 3.1 inspection certificate. Aktif Çelik supplies 1.4401 / 316 (1.4404 / 316L on request) round, hexagon, square and flat bars to EN 10088-3 or ASTM A276 / A479, from stock or from production partners; stock status for the size, minimum quantity and lead time vary by product and are stated in the quotation. Third-party inspection (e.g. SGS, Bureau Veritas, TÜV) is arranged on request.

Related technical article: X2CrNiMo17-12-2

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
ENX2CrNiMo17-12-2
W.-Nr. (DIN)1.4404
AISI / UNS316L / S31603
ASTMA182 F316L · A276 · A240
JISSUS316L
GOST≈ 03Х17Н14М3 (03Kh17N14M3)
AFNORZ3CND17-11-02 / Z2CND17-12
BS (UK)316S11
GB (China)022Cr17Ni12Mo2

Steel Equivalence Tables

Detailed comparison: 304 vs 316L · 316L vs 1.4404

Applications

  • Chemical and petrochemical plants
  • Pharmaceutical and medical equipment parts
  • Food and beverage equipment
  • Flanges, fittings and valve parts
  • Heat exchangers and process piping
  • Marine hardware (above-water service)

Frequently Asked Questions

Are 316L and 1.4404 the same?+

In practice they are the ASTM/AISI and EN designations of the same material, but the ranges do not fully overlap: EN 1.4404 has Mo 2.00–2.50%, ASTM 316L 2.00–3.00%, and the Ni and Cr ranges differ slightly as well. See our 316L vs 1.4404 page for a detailed comparison. Dual-certified material is common.

What is the difference between 316 and 316L?+

316 (1.4401) is the version with carbon ≤ 0.07%; 316L (1.4404) limits carbon to ≤ 0.030%. Low carbon reduces chromium carbide precipitation during welding and lowers the risk of intergranular corrosion in welded parts. The F316/F316L dual certification common on flanges and fittings shows that the material meets the requirements of both grades.

1.4404 or 1.4571 (316Ti)?+

1.4571 is a molybdenum grade in which carbon is tied up (stabilised) by titanium; it is widespread in German-speaking markets. 1.4404 achieves the same aim by lowering carbon. In most aqueous corrosive media they behave similarly; titanium carbonitrides in 1.4571 limit polishability, so 1.4404 is usually preferred where a bright, polished surface is required. The project specification decides which one is used.

Can 316L be used in seawater?+

It is widely used for above-water and splash-zone hardware. However, when continuous seawater contact, stagnant water, crevices and elevated temperature combine, pitting and crevice corrosion can also occur on 316L. Under such conditions duplex (1.4462) or super-austenitic and super-duplex grades are considered.

Does Aktif Çelik supply 316L stainless bars?+

1.4401 / 316 round, hexagon, square and flat bars are supplied with an EN 10204 3.1 certificate; 1.4404 / 316L or dual-certified 316/316L material is quoted on request. Whether a given size is in stock, the minimum quantity and the lead time are stated in the quotation.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools