Steel Equivalence Tables

GOST – EN steel equivalents

In Russia and the CIS countries, steel is identified by the grade names of the GOST standards: 38ХМ, 40ХН, steel 45, ШХ15. This page shows the nearest GOST equivalents of the EN grades on this site and explains how GOST names are read.

GOST – EN – AISI equivalence table

Click a grade name to open its datasheet.

ENW.-Nr.GOSTStandardAISI/SAE
42CrMo41.7225≈ 38ХМ (38KhM)GOST 45434140
C451.050345GOST 10501045
S235JR1.0038≈ Ст3сп (St3sp)GOST 380≈ A36
S355J21.0577≈ 09Г2С (09G2S)GOST 19281≈ A572 Gr.50
16MnCr51.7131≈ 18ХГТ (18KhGT)GOST 45435115
34CrNiMo61.6582≈ 38ХН3МА (38KhN3MA)GOST 4543≈ 4340
100Cr61.3505ШХ15 (ShKh15)GOST 80152100
C151.0401≈ Сталь 15GOST 1050≈ 1015 / 1018
20NiCrMo2-21.6523≈ 20ХНМ (20KhNM)—8620
51CrV41.8159≈ 50ХФА (50KhFA)GOST 149596150
39NiCrMo31.6510≈ 40ХН (40KhN)GOST 4543≈ 9840
20MnCr51.7147≈ 18ХГТ (18KhGT)GOST 45435120
41Cr41.7035≈ 40Х (40Kh)—≈ 5140
C351.050135 (сталь 35)—≈ 1035
C401.051140 (сталь 40)—≈ 1040
34CrMo41.7220≈ 35ХМ (35KhM)—≈ 4135
C601.0601≈ 60 (сталь 60)—≈ 1060
C22E1.1151≈ 20 (сталь 20)—≈ 1020
X5CrNi18-101.4301≈ 08Х18Н10 (08Kh18N10)—304
X2CrNiMo17-12-21.4404≈ 03Х17Н14М3 (03Kh17N14M3)—316L
E2951.0050≈ Ст5сп (St5sp)——
55Cr31.7176≈ 50ХГА (50KhGA)—≈ 5155 / 5160
60Si71.5027≈ 60С2 (60S2)—≈ 9260
C551.0535≈ 55 (сталь 55)GOST 1050≈ 1055

Equivalents are given for information; analysis ranges may differ slightly from one standard to another. For critical parts, the standard named in your order governs. “≈” marks the nearest grade where no strict equivalent exists.

Rows are generated from the same data as the steel grade datasheets on this site.

How to read GOST grade names

  • The first two digits are the carbon content in hundredths of a percent: 38ХМ → about 0.38 % C; 45 → 0.45 % C.
  • Letters stand for alloying elements: Х chromium, Н nickel, М molybdenum, Г manganese, С silicon, Ф vanadium, Т titanium, Ю aluminium, Р boron.
  • With no number after a letter, the element is present up to about 1.5 %; a number gives the approximate percentage: 38ХН3МА → ≈ 3 % Ni.
  • A final А marks a high-quality steel with lower sulphur and phosphorus: 50ХФА, 38ХН3МА.
  • Ст3сп: general-purpose carbon structural steel to GOST 380; сп = killed, пс = semi-killed, кп = rimming steel.
  • ШХ15: bearing steel (GOST 801); Ш = bearing, Х15 = ≈ 1.5 % Cr. А20: free-cutting steel (GOST 1414).

You can send your enquiry using the GOST designation; we confirm the EN counterpart.

Send us your requirements