Steel Grade Datasheet

E295/ 1.0050Non-Alloy Engineering Steel (EN 10025-2)

Standard
EN 10025-2
Delivery Conditions
+AR, +N
Density
7.85 g/cm³
W.-Nr.
1.0050

What is E295 steel?

E295 (Werkstoff No. 1.0050, old DIN name St 50-2) is a non-alloy engineering steel defined in EN 10025-2. The E stands for engineering steel and 295 is the minimum yield strength in MPa guaranteed up to 16 mm thickness. Tensile strength is 470–610 MPa for 3–100 mm. The standard only limits P, S and N; carbon, silicon and manganese are not specified. That is why it is used for machined parts such as shafts, axles and pins, and why its weldability is not guaranteed.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C / Si / Mn—
P≤ 0.045
S≤ 0.045
N≤ 0.012

Mechanical Properties (+AR / +N)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 16295470–61020
16 < d ≤ 40285470–61020
40 < d ≤ 63275470–61019
63 < d ≤ 80265470–61018
80 < d ≤ 100255470–61018
100 < d ≤ 150245450–61016
150 < d ≤ 200235440–61015
200 < d ≤ 250225440–61015

Hardness: EN 10025-2 does not specify hardness. A tensile strength of 470–610 MPa corresponds to roughly 140–180 HB (approximate conversion, not a standard value).

E295 / 1.0050 properties and use

E295 is the lowest-strength of the three engineering steels in EN 10025-2 (E295, E335, E360). It differs from the S grades (S235, S275, S355) in purpose: S grades are defined for welded steel structures by chemical composition, carbon equivalent and impact energy, whereas E295 only has limits for phosphorus (≤ 0.045%), sulphur (≤ 0.045%) and nitrogen (≤ 0.012%) and no impact test requirement. It is mostly used as hot-rolled round, square and flat bar and as plate; according to a note in the standard it is not usually used for channels, angles and sections. The cold-drawn counterpart for bright bars is E295GC in EN 10277. Yield strength falls with thickness: 295 MPa up to 16 mm, 285 MPa at 16–40 mm, 265 MPa at 63–80 mm and 225 MPa at 200–250 mm. Since carbon is not limited, if welding is required the carbon equivalent should be calculated from the actual analysis (3.1 certificate) and preheating assessed. For parts that need quenching and tempering or surface hardening, grades with a defined composition such as C35, C45 or 42CrMo4 are more suitable. For a quotation, state the product shape (round, flat, plate), size, length, quantity and, if needed, the delivery condition (+AR, +N). Aktif Çelik reviews the request through its supply network and prepares a quote; the material can be requested with an EN 10204 3.1 inspection certificate.

Related technical article: E295

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
ENE295
W.-Nr. (DIN)1.0050
DIN 17100 (old)St 50-2
AISI/SAE—
AFNOR≈ A50-2
UNI≈ Fe 490-2
JIS≈ SS490
GOST≈ Ст5сп (St5sp)

Steel Equivalence Tables

Applications

  • Shafts and axles
  • Pins, bolt blanks and studs
  • Lightly loaded gears and gear blanks
  • Keys, levers and linkage parts
  • Agricultural machinery parts
  • Machined parts for general engineering

Frequently Asked Questions

Are E295 and St 50-2 the same steel?+

Yes. St 50-2 is the old name from DIN 17100, and the material number is 1.0050 in both cases. DIN 17100 was replaced by EN 10025 (where the grade was first called Fe 490-2) and later by EN 10025-2, where it is E295. If an old drawing says St 50-2, you can order E295 to EN 10025-2.

Can E295 be welded?+

The standard sets no carbon or carbon-equivalent limit for E295 and no impact test, so its weldability is not guaranteed. If welding is unavoidable, calculate the carbon equivalent from the actual analysis on the 3.1 certificate and choose preheating and welding procedure accordingly. For welded load-bearing structures, S grades such as S355J2 are preferred.

E295, S355J2 or C45: which one?+

Choose S355J2 for welded steel structures with an impact requirement at −20 °C; C45, with its defined composition, for parts whose strength will be raised by heat treatment (quenching and tempering, induction hardening); and E295 for unwelded machined parts where a yield strength of around 295 MPa is sufficient. E295 has a lower yield strength than S355J2 and no impact requirement.

Does E295 carry CE marking?+

Within the EN 10025 series, CE marking applies to structural steels; the engineering steels E295, E335 and E360 are excluded from it. Conformity of E295 is therefore shown with an EN 10204 inspection document against the ordered standard.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).