Steel Grade Datasheet

C35/ 1.0501 / ≈ 1035Medium-Carbon Steel for Quenching and Tempering

Standard
EN 10083-2
Delivery Conditions
+A, +N, +QT
Density
7.85 g/cm³
W.-Nr.
1.0501

What is C35 steel?

C35 (material no. 1.0501) is a non-alloy medium-carbon steel for quenching and tempering to EN 10083-2, with 0.32–0.39% carbon and 0.50–0.80% manganese. Quenched and tempered (+QT), it reaches a minimum yield strength of 430 MPa and a tensile strength of 630–780 MPa up to 16 mm; in the 40–100 mm range the values fall to 320 MPa and 550–700 MPa. Its direct GOST counterpart is steel 35; AISI 1035 and JIS S35C are the nearest matches.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.32–0.39
Si≤ 0.40
Mn0.50–0.80
P≤ 0.045 (C35E/C35R ≤ 0.030)
S≤ 0.045 (C35E ≤ 0.035; C35R 0.020–0.040)
Cr≤ 0.40
Mo≤ 0.10
Ni≤ 0.40
Cr+Mo+Ni≤ 0.63

Mechanical Properties (+QT)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 16430630–78017
16 < d ≤ 40380600–75019
40 < d ≤ 100320550–70020

Mechanical Properties (+N)

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 16300≥ 55018
16 < d ≤ 100270≥ 52019
100 < d ≤ 250245≥ 50019

Hardness: +QT: Rm 550–780 MPa ≈ 165–230 HB · +N: Rm ≥ 500–550 MPa · HB values are an approximate conversion per EN ISO 18265; EN 10083-2 specifies strength, not hardness, for +N/+QT.

C35 / 1.0501 properties and use

C35 sits between the low-carbon C22 and the widely used C45. With less carbon than C45 it is tougher, easier to cold-form and more forgiving to weld, but it reaches lower strength and surface hardness after hardening. As a non-alloy steel its hardenability is limited: in larger sections mainly the near-surface zone hardens, which is why the EN 10083-2 tensile range drops from 630–780 MPa at 16 mm to 550–700 MPa at 100 mm. Where high strength is needed through the whole section, a Cr or CrMo grade such as 41Cr4 or 34CrMo4 is the better choice. EN 10083-2 defines three versions with identical mechanical values: C35 (1.0501); C35E (1.1181) with tighter phosphorus and sulphur limits — the successor of the old DIN grade Ck35; and C35R (1.1180) with a controlled sulphur range of 0.020–0.040% for better machinability. Guideline heat treatment: normalizing at about 860–900 °C, hardening from about 840–880 °C in water or polymer, tempering at 550–660 °C. Delivery conditions are untreated, soft annealed (+A), normalized (+N) or quenched and tempered (+QT). Weldability is fair: thin sections weld without difficulty, while preheating for thicker sections should be set in the welding procedure according to carbon equivalent and thickness. Aktif Çelik quotes C35 through its supply network as hot-rolled or bright bar and as forgings; size, delivery condition, quantity and lead time are confirmed in the quotation, and deliveries can be made with an EN 10204 3.1 inspection certificate.

Related technical article: C35

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
ENC35
W.-Nr. (DIN)1.0501
EN (E / R)C35E 1.1181 / C35R 1.1180
DIN 17200 (old)Ck35 (= C35E)
AISI/SAE≈ 1035
JIS≈ S35C
GOST35 (сталь 35)
GB (China)35

Steel Equivalence Tables

Applications

  • Moderately stressed shafts, axles and pins
  • Bolts, studs and fasteners
  • Forgings for general mechanical engineering
  • Gears and couplings under moderate load
  • Levers, hubs and connecting parts
  • Hydraulic and agricultural machinery components

Frequently Asked Questions

What is the difference between C35 and C45?+

C45 contains about 0.10% more carbon (0.42–0.50% versus 0.32–0.39%). Quenched and tempered up to 16 mm, C45 gives 700–850 MPa and C35 630–780 MPa tensile strength, and C45 also reaches a higher surface hardness after induction hardening. C35 is tougher, more ductile and easier to weld. Choose C35 where moderate strength must go with toughness or weldability, and C45 where strength and wear resistance come first.

Is C35 the same as GOST steel 35 and AISI 1035?+

GOST 1050 steel 35 (0.32–0.40% C, 0.50–0.80% Mn) is a direct counterpart. AISI/SAE 1035 and JIS S35C are close but not identical: both specify 0.32–0.38% C and 0.60–0.90% Mn. For certified supply, the standard named in the order governs.

What do C35E, C35R and Ck35 mean?+

C35E (1.1181) limits phosphorus to ≤ 0.030% and sulphur to ≤ 0.035%; its old DIN 17200 name is Ck35. C35R (1.1180) contains 0.020–0.040% sulphur for better chip breaking. All three versions share the same mechanical values, so state the exact designation on the order.

Can C35 be welded and surface hardened?+

Yes. For welding, preheating of thicker sections is set in the welding procedure. Flame or induction hardening is possible, but because of its lower carbon content C35 does not reach the surface hardness that C45 achieves with the same treatment.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).