Steel Grade Datasheet

C40/ 1.0511 / ≈ 1040Medium-Carbon Steel for Quenching and Tempering

Standard
EN 10083-2
Delivery Conditions
+A, +N, +QT
Density
7.85 g/cm³
W.-Nr.
1.0511

What is C40 steel?

C40 (material no. 1.0511) is a non-alloy medium-carbon steel for quenching and tempering to EN 10083-2, with 0.37–0.44% carbon and 0.50–0.80% manganese. Quenched and tempered (+QT), it offers a minimum yield strength of 460 MPa and 650–800 MPa tensile strength up to 16 mm, and 350 MPa / 600–750 MPa for 40–100 mm. Its direct GOST counterpart is steel 40; the British EN8 (BS 970 080M40) and AISI 1040 are the nearest matches.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.37–0.44
Si≤ 0.40
Mn0.50–0.80
P≤ 0.045 (C40E/C40R ≤ 0.030)
S≤ 0.045 (C40E ≤ 0.035; C40R 0.020–0.040)
Cr≤ 0.40
Mo≤ 0.10
Ni≤ 0.40
Cr+Mo+Ni≤ 0.63

Mechanical Properties (+QT)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 16460650–80016
16 < d ≤ 40400630–78018
40 < d ≤ 100350600–75019

Mechanical Properties (+N)

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 16320≥ 58016
16 < d ≤ 100290≥ 55017
100 < d ≤ 250260≥ 53017

Hardness: +QT: Rm 600–800 MPa ≈ 180–240 HB · +N: Rm ≥ 530–580 MPa · HB values are an approximate conversion per EN ISO 18265; EN 10083-2 specifies strength, not hardness, for +N/+QT.

C40 / 1.0511 properties and use

C40 sits between C35 and C45: it gives more strength and surface hardness than C35 and slightly better toughness and weldability than C45. As a non-alloy steel its hardenability is limited, so the EN 10083-2 values fall as the section grows and the table ends at 100 mm. For larger sections, or parts that need strength through the full section, an alloy grade such as 41Cr4 or 42CrMo4 should be chosen. In the UK and India bars are still often ordered as 'EN8' (BS 970 080M40, 0.36–0.44% C). Among EN 10083-2 grades, C40 has the closest carbon range, although C45 is also commonly offered against EN8 enquiries — so the governing standard should be stated on the order. EN 10083-2 also lists C40E (1.1186; P ≤ 0.030%, S ≤ 0.035%) and C40R (1.1189; S 0.020–0.040%) with the same mechanical values. Guideline heat treatment: normalizing at about 850–890 °C, hardening from about 830–870 °C in water or polymer, tempering at 550–660 °C. C40 is suitable for flame and induction hardening and is used for pins, journals and guide surfaces. For welding, preheating of thicker sections should be set in the welding procedure. Aktif Çelik quotes C40 through its supply network as hot-rolled and bright (cold-drawn or peeled) bar; size, delivery condition, quantity and lead time are confirmed in the quotation, and deliveries can be made with an EN 10204 3.1 inspection certificate.

Related technical article: C40

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
ENC40
W.-Nr. (DIN)1.0511
EN (E / R)C40E 1.1186 / C40R 1.1189
AISI/SAE≈ 1040
JIS≈ S40C
GOST40 (сталь 40)
BS 970 (UK)≈ 080M40 (EN8)
GB (China)40

Steel Equivalence Tables

Applications

  • Shafts, axles and spindles
  • Induction-hardened pins and journals
  • Bolts, studs and nuts
  • Gears and sprockets under moderate load
  • Hydraulic cylinder and machine components
  • Forged machine elements

Frequently Asked Questions

Is C40 the same as EN8 (080M40)?+

Close, but not identical. BS 970 080M40 specifies 0.36–0.44% C and 0.60–1.00% Mn, while C40 has 0.37–0.44% C and 0.50–0.80% Mn. Because the two standards define the mechanical requirements differently, the order should name one governing standard (e.g. 'C40 to EN 10083-2, equivalent to EN8').

Should I choose C40 or C45?+

C45 has about 0.05% more carbon. Quenched and tempered up to 16 mm, C40 gives 650–800 MPa and C45 700–850 MPa tensile strength. Choose C45 for higher strength and surface hardness, and C40 for slightly more toughness and easier welding.

What are C40E and C40R?+

C40E (1.1186) limits phosphorus to ≤ 0.030% and sulphur to ≤ 0.035%; C40R (1.1189) contains 0.020–0.040% sulphur for chip breaking. Their mechanical values are the same as base C40.

Can C40 be induction hardened?+

Yes. As a medium-carbon steel, C40 responds to flame and induction hardening and is used for wearing surfaces such as pins and journals. The surface hardness reached depends on the process and stays somewhat below C45 for the same treatment.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).