What is 41Cr4 steel?

41Cr4 (material no. 1.7035) is a chromium alloy steel for quenching and tempering to EN 10083-3, with 0.38–0.45% carbon, 0.60–0.90% manganese and 0.90–1.20% chromium. Quenched and tempered (+QT), it offers a minimum yield strength of 800 MPa and 1000–1200 MPa tensile strength up to 16 mm, and 560 MPa / 800–950 MPa for 40–100 mm. Its nearest counterparts are AISI 5140, JIS SCr440 and GOST 40Kh (40Х).

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.38–0.45
Si≤ 0.40
Mn0.60–0.90
P≤ 0.025
S≤ 0.035 (41CrS4: 0.020–0.040)
Cr0.90–1.20

Mechanical Properties (+QT)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 168001000–120011
16 < d ≤ 40660900–110012
40 < d ≤ 100560800–95014

Hardness: +QT: Rm 800–1200 MPa ≈ 240–355 HB · HB values are an approximate conversion per EN ISO 18265; EN 10083-3 specifies strength, not hardness, for +QT · +A (soft annealed) for machining.

41Cr4 / 1.7035 properties and use

Chromium lifts the hardenability of 41Cr4 well above that of non-alloy C45, so higher strength is reached in medium sections after quenching and tempering. Without molybdenum it is more economical than 42CrMo4, but its hardenability is lower: EN 10083-3 gives values only up to 100 mm. Molybdenum-free chromium steels are also more prone to temper embrittlement when cooled slowly after tempering, which is why 42CrMo4 is usually preferred for large sections and toughness-critical parts. Machining is done in the soft annealed (+A) condition; the variant 41CrS4 (1.7039), with sulphur held at 0.020–0.040%, improves machinability. Guideline heat treatment: hardening from about 820–860 °C in oil or water and tempering at 540–680 °C. 41Cr4 is well suited to flame and induction hardening and is used this way for wearing journals, pins and gear surfaces. Weldability is limited: if welding is required, preheating and post-weld heat treatment must follow a qualified procedure. Aktif Çelik quotes 41Cr4 through its supply network as hot-rolled round bar, bright (peeled or cold-drawn) bar and as forgings; size, delivery condition, quantity and lead time are confirmed in the quotation, and deliveries can be made with an EN 10204 3.1 inspection certificate.

Related technical article: 41Cr4

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
EN41Cr4
W.-Nr. (DIN)1.7035
EN (S)41CrS4 1.7039
AISI/SAE≈ 5140
JIS≈ SCr440
GOST≈ 40Х (40Kh)
AFNOR (old)≈ 42C4
BS 970 (UK)≈ 530M40 (EN18)
GB (China)≈ 40Cr

Steel Equivalence Tables

Applications

  • Axle shafts and steering components
  • Gears and pinions under moderate load
  • High-strength bolts, studs and nuts
  • Induction-hardened shafts, pins and journals
  • Forged machine parts
  • Crank and connecting elements

Frequently Asked Questions

What is the difference between 41Cr4 and 42CrMo4?+

Both have the same carbon range (0.38–0.45%); 42CrMo4 additionally contains 0.15–0.30% molybdenum. Molybdenum increases hardenability and reduces temper embrittlement: 42CrMo4 values are given up to 250 mm and reach 1100–1300 MPa at 16 mm, whereas the 41Cr4 table ends at 100 mm with 1000–1200 MPa at 16 mm. 41Cr4 is an economical choice for medium sections; 42CrMo4 is preferred for large ones.

Is 41Cr4 the same as GOST 40Kh (40Х) and AISI 5140?+

Close, but not identical. GOST 4543 grade 40Х has 0.36–0.44% C, 0.50–0.80% Mn and 0.80–1.10% Cr; AISI 5140 specifies 0.38–0.43% C, 0.70–0.90% Mn and 0.70–0.90% Cr, i.e. less chromium. The closest in composition is JIS SCr440. For certified supply, the standard named in the order governs.

Can 41Cr4 be induction hardened?+

Yes. 41Cr4 is a classic steel for flame and induction hardening, usually as a hardened surface on a quenched-and-tempered core for shafts, pins and journals. The surface hardness and depth reached depend on the process.

In which delivery conditions is 41Cr4 available?+

EN 10083-3 allows delivery untreated, treated for shearability (+S), soft annealed (+A) or quenched and tempered (+QT). Choose +A for machining and +QT for direct use; if machinability matters, the 41CrS4 variant can be specified.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).