Steel Grade Datasheet

55Cr3/ 1.7176 / ≈ 5155 / 5160Chromium Spring Steel (EN 10089)

Standard
EN 10089
Delivery Conditions
+AR, +S, +A, +AC
Density
7.85 g/cm³
W.-Nr.
1.7176

What is 55Cr3 steel?

55Cr3 (Werkstoff No. 1.7176) is a quench-and-temper spring steel defined in EN 10089, with 0.52–0.59% carbon and 0.70–1.00% chromium. Its chemically closest US counterpart is SAE 5155, although buyers often ask for it as an SAE 5160 equivalent. According to the guidance values in EN 10089 Annex D, oil quenching from 840 °C and tempering at 400 °C give Rp0.2 ≥ 1250 MPa and Rm 1400–1700 MPa. It is used for truck and trailer leaf springs, coil springs and anti-roll bars.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.52–0.59
Si≤ 0.40
Mn0.70–1.00
P≤ 0.025
S≤ 0.025
Cr0.70–1.00

Mechanical Properties (+QT · EN 10089)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
Ref. +QT12501400–17003

Hardness: +A ≤ 248 HB · +S ≤ 280 HB · +AC ≤ 230 HB (EN 10089). After quenching and tempering (Annex D guidance) Rm 1400–1700 MPa, roughly 44–50 HRC (approximate conversion).

55Cr3 / 1.7176 properties and use

55Cr3 is a chromium-manganese spring steel with silicon kept low (≤ 0.40%). Chromium raises hardenability; without vanadium it suits thinner sections than 51CrV4. Per EN 10089 Table 5 (upper 2/3 of the hardenability band, oil quenching, 80% martensite at the core) the maximum size is 28 mm for rounds and 20 mm for flats; under the same conditions 51CrV4 reaches 54 mm and 39 mm. For thick leaves and large-diameter bars, 51CrV4 or grades with higher hardenability are therefore considered. Standard delivery conditions are as rolled (+AR), treated to improve shearability (+S, ≤ 280 HB), soft annealed (+A, ≤ 248 HB) and annealed to spheroidise the carbides (+AC, ≤ 230 HB). The spring maker forms the material and carries out the quenching and tempering, so chemical analysis, hardenability (if needed the +H/+HH bands), surface decarburisation and surface quality are decisive in the order. The standard does not permit surface defects to be removed by welding. For a quotation, state the product shape (flat or round), size and tolerance, length, quantity, delivery condition and any hardenability requirement. Aktif Çelik reviews the request through its supply network and prepares a quote; the material can be requested with an EN 10204 3.1 inspection certificate.

Related technical article: 55Cr3

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
EN55Cr3
W.-Nr. (DIN)1.7176
AISI/SAE≈ 5155 / 5160
JIS≈ SUP9
GOST≈ 50ХГА (50KhGA)
BS (UK)≈ 527A60
GB (China)≈ 55CrMnA

Steel Equivalence Tables

Applications

  • Truck and trailer leaf (parabolic) springs
  • Coil springs
  • Anti-roll (stabiliser) bars
  • Small-section torsion bars
  • Spring elements for agricultural machinery
  • General engineering springs

Frequently Asked Questions

Is 55Cr3 the same as SAE 5160?+

Not exactly. Chemically, the closest SAE grade to 55Cr3 is 5155 (C 0.51–0.59%). SAE 5160 has slightly more carbon (0.56–0.64%); in EN 10089 the grade closest to 5160 is 60Cr3 (1.7177, C 0.55–0.65%). If a drawing calls for SAE 5160, confirm the carbon range of a 55Cr3 alternative with the buyer.

55Cr3 or 51CrV4?+

Choose by section and load. 55Cr3 has lower hardenability: per EN 10089 it is suitable up to about 28 mm diameter for 80% martensite at the core, 51CrV4 up to about 54 mm. Thanks to vanadium, 51CrV4 is fine-grained and more fatigue resistant, so it is preferred for thick leaves and highly stressed springs. For thinner sections 55Cr3 is a common choice.

What hardness is 55Cr3 tempered to?+

It depends on the application. The guidance heat treatment in EN 10089 Annex D (840 °C oil, 400 °C tempering) gives Rp0.2 ≥ 1250 MPa, Rm 1400–1700 MPa, A ≥ 3% and Z ≥ 20%, roughly 44–50 HRC. The exact hardness is set by the tempering temperature to suit the spring design.

Can 55Cr3 be welded?+

Welding is not recommended for a spring steel: the high carbon forms a hard, brittle zone at the weld and reduces fatigue life. EN 10089 also does not permit surface defects to be removed by welding. Connections are made by bolting, clamping or hot forming.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

References & Standards

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).