Steel Grade Datasheet

60Si7/ 1.5027 / ≈ 9260Silicon-Manganese Spring Steel

Standard
EURONORM 89
Delivery Conditions
+AR, +A
Density
≈ 7.80 g/cm³
W.-Nr.
1.5027

What is 60Si7 steel?

60Si7 (Werkstoff No. 1.5027) is a silicon-manganese spring steel with 0.57–0.64% carbon and 1.50–2.00% silicon. It is defined in EURONORM 89 and the national standards based on it; it is not part of the current EN 10089, where the closest grades are 56Si7 (1.5026) and 61SiCr7 (1.7108). In the quenched and tempered reference condition its tensile strength is 1373–1618 MPa with at least 5% elongation. Close counterparts are GOST 60S2 (60С2), SAE 9260 and Chinese 60Si2Mn. It is used for thin-section leaf and coil springs.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.57–0.64
Si1.50–2.00
Mn0.60–0.90
P≤ 0.040
S≤ 0.040

Mechanical Properties (+QT · EU 89)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
Ref. +QT—1373–16185

Hardness: After quenching and tempering (EU 89 reference) Rm 1373–1618 MPa, roughly 43–49 HRC (approximate conversion). Annealed delivery hardness depends on the ordering standard; for 56Si7 in EN 10089 it is +A ≤ 248 HB, +S ≤ 280 HB.

60Si7 / 1.5027 properties and use

60Si7 originates from EURONORM 89 and the national standards based on it (e.g. DIN 17221); it is not included in EN 10089, published in 2002. National versions differ slightly (some DIN records give C 0.56–0.64% and Mn 0.70–1.00%), so the order should state which standard applies. If an old drawing calls for 60Si7, substitution by 56Si7 from EN 10089 (C 0.52–0.60%, Si 1.60–2.00%) or by the chromium-bearing 61SiCr7 (C 0.57–0.65%, Si 1.60–2.00%, Cr 0.20–0.45%) is agreed with the buyer. Silicon raises the elastic limit and resistance to setting, but makes the steel prone to surface decarburisation during heating. Without chromium, hardenability is limited: per EN 10089 Table 5, the nearest grade 56Si7 achieves 80% martensite at the core on oil quenching up to 11 mm for rounds and 8 mm for flats (61SiCr7: 21 mm and 15 mm). EN 10089 Annex D gives 860 °C oil quenching and 450 °C tempering as the guidance heat treatment for 56Si7. For a quotation, state the governing standard (EURONORM 89, a national standard or an EN 10089 substitute), product shape, size and tolerance, length, quantity and decarburisation limit. Aktif Çelik reviews the request through its supply network and prepares a quote; the material can be requested with an EN 10204 3.1 inspection certificate.

Related technical article: 60Si7

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
EN 10089≈ 56Si7 (1.5026) / 61SiCr7 (1.7108)
W.-Nr. (DIN)1.5027
AISI/SAE≈ 9260
JIS≈ SUP6 / SUP7
GOST≈ 60С2 (60S2)
GB (China)≈ 60Si2Mn

Steel Equivalence Tables

Applications

  • Thin-section leaf springs
  • Small-section coil springs
  • Spring clips and retaining elements
  • Spring elements for agricultural machinery
  • Formed (shaped) springs
  • General engineering springs

Frequently Asked Questions

Which standard covers 60Si7, and is it in EN 10089?+

60Si7 (1.5027) is a spring steel designation defined in EURONORM 89 and some national standards (e.g. DIN 17221); it is not included in the current EN 10089:2002. The closest EN 10089 grades are 56Si7 (1.5026) and the chromium-bearing 61SiCr7 (1.7108). If a drawing says 60Si7, agree the governing standard and any acceptable substitute with the buyer before ordering.

What is the GOST equivalent of 60Si7?+

The closest is 60S2 (60С2) to GOST 14959: with C 0.57–0.65%, Si 1.50–2.00% and Mn 0.60–0.90% it is very close to the EURONORM 89 composition of 60Si7. Close grades elsewhere are 60Si2Mn in China, SAE 9260 in the US and SUP6/SUP7 in Japan; none is identical.

What does silicon do in a spring steel?+

Silicon strengthens the ferrite, raising the elastic limit and the resistance to setting (relaxation) under load, which is why steels with 1.5–2% Si are common in leaf and coil springs. The drawback is a tendency to lose carbon at the surface during heating. Because a decarburised surface layer lowers fatigue life, the order should specify a decarburisation limit.

What section sizes is 60Si7 suitable for?+

Silicon-manganese spring steels without chromium have low hardenability. EN 10089 Table 5 gives, for the nearest grade 56Si7, a maximum size of 11 mm for rounds and 8 mm for flats for 80% martensite at the core after oil quenching; for 61SiCr7 the values are 21 mm and 15 mm. Thicker sections use grades with higher hardenability such as 51CrV4.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

References & Standards

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).