Steel Grade Datasheet

30CrNiMo8/ 1.6580Ni-Cr-Mo Steel for Quenching and Tempering (High Hardenability)

Standard
EN 10083-3
Delivery Conditions
+A, +QT
Density
7.85 g/cm³
W.-Nr.
1.6580

What is 30CrNiMo8 steel?

30CrNiMo8 (material no. 1.6580) is a nickel-chromium-molybdenum steel for quenching and tempering to EN 10083-3, with 0.26–0.34% C, 1.80–2.20% Cr, 1.80–2.20% Ni and 0.30–0.50% Mo. Quenched and tempered (+QT), it reaches a minimum yield strength of 1050 MPa and 1250–1450 MPa tensile strength up to 40 mm, and still 700 MPa / 900–1100 MPa in sections of 160–250 mm. It is chosen for large, heavily loaded parts that need high strength and toughness through the whole section.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.26–0.34
Si≤ 0.40
Mn0.50–0.80
P≤ 0.025
S≤ 0.035
Cr1.80–2.20
Mo0.30–0.50
Ni1.80–2.20

Mechanical Properties (+QT)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 1610501250–14509
16 < d ≤ 4010501250–14509
40 < d ≤ 1009001100–130010
100 < d ≤ 1608001000–120011
160 < d ≤ 250700900–110012

Hardness: +QT: Rm 900–1450 MPa ≈ 265–425 HB · HB values are an approximate conversion per EN ISO 18265; EN 10083-3 specifies strength, not hardness, for +QT · +A (soft annealed) for machining.

30CrNiMo8 / 1.6580 properties and use

With roughly 4–5% Cr, Ni and Mo combined, 30CrNiMo8 has very high hardenability: in the EN 10083-3 table it exceeds 34CrNiMo6 in every size range (e.g. 900–1100 MPa versus 800–950 MPa at 160–250 mm). The moderate carbon content keeps toughness high, nickel improves toughness further and molybdenum provides resistance to temper embrittlement. Large parts are usually rough-machined in the soft annealed (+A) condition, then quenched and tempered and finish-machined; for large forgings, controlled cooling after forging and a defined heat-treatment route are important. Guideline heat treatment: hardening from about 830–860 °C in oil and tempering at 540–660 °C. There is no direct AISI/SAE or JIS equivalent; the old French designation 30CND8 is the closest match. When comparing with US NiCrMo grades such as 4340, compare required properties and section size rather than names. Because of its high hardenability, welding is generally avoided. Aktif Çelik quotes 30CrNiMo8 through its supply network as forged bar, hot-rolled round bar and forgings; size, delivery condition, quantity and lead time are confirmed in the quotation, and deliveries can be made with an EN 10204 3.1 inspection certificate.

Related technical article: 30CrNiMo8

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
EN30CrNiMo8
W.-Nr. (DIN)1.6580
AFNOR (old)≈ 30CND8

Steel Equivalence Tables

Applications

  • Heavily loaded drive and transmission shafts
  • Large-section gears and pinions
  • Heavy-machinery forgings (crank and connecting parts)
  • Large-diameter high-strength bolts and studs
  • Mining and construction equipment components
  • Couplings and torsion-loaded parts

Frequently Asked Questions

What is the difference between 30CrNiMo8 and 34CrNiMo6?+

30CrNiMo8 contains more chromium (1.80–2.20% vs 1.30–1.70%), nickel (1.80–2.20% vs 1.30–1.70%) and molybdenum (0.30–0.50% vs 0.15–0.30%) but less carbon (0.26–0.34% vs 0.30–0.38%). The result is higher strength in every size range: 1250–1450 vs 1200–1400 MPa up to 16 mm, and 900–1100 vs 800–950 MPa at 160–250 mm. 34CrNiMo6 is more widely used and usually more economical.

Is there an AISI equivalent of 30CrNiMo8?+

There is no direct one. The old French grade 30CND8 is the closest match. US NiCrMo steels such as 4340 differ in carbon and alloy balance, so any substitution should be based on the required properties and section size and approved by the design engineer.

Can 30CrNiMo8 be welded?+

Welding is generally avoided because of its high hardenability and the risk of cold cracking. If it cannot be avoided, a qualified procedure with preheating, controlled interpass temperature and post-weld heat treatment is required.

How is 30CrNiMo8 supplied and machined?+

Choose soft annealed (+A) for machining and quenched and tempered (+QT) for direct use. Large parts are usually rough-machined in +A, then quenched and tempered and brought to final size, so that heat-treatment distortion is removed in finish machining.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

References & Standards

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).