Steel Grade Datasheet

18CrNiMo7-6/ 1.6587Ni-Cr-Mo Case-Hardening Steel

Standard
EN ISO 683-3
Delivery Conditions
+A, +FP
Density
7.85 g/cm³
W.-Nr.
1.6587

What is 18CrNiMo7-6 steel?

18CrNiMo7-6 (material no. 1.6587, formerly 17CrNiMo6) is a nickel-chromium-molybdenum case-hardening steel to EN ISO 683-3 (formerly EN 10084), with 0.15–0.21% C, 1.50–1.80% Cr, 1.40–1.70% Ni and 0.25–0.35% Mo. After carburizing, hardening and low-temperature tempering it combines a hard, wear-resistant case with a tough, strong core, even in large sections. It is widely used for large, heavily loaded gears, for example in industrial and wind-turbine gearboxes.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.15–0.21
Si≤ 0.40
Mn0.50–0.90
P≤ 0.025
S≤ 0.035
Cr1.50–1.80
Mo0.25–0.35
Ni1.40–1.70

Mechanical Properties

Hardness by Delivery Condition

Hardness limits given by the standard for these delivery conditions; certified values are stated on the inspection certificate (EN 10204 3.1).

Delivery conditionHardness
+A≤ 229 HB
+FP159–207 HB

Hardness: +A: ≤ 229 HB · +FP: 159–207 HB (EN ISO 683-3) · Carburized and hardened surface: typically 58–62 HRC, process-dependent

18CrNiMo7-6 / 1.6587 properties and case hardening

Compared with the MnCr case-hardening steels 16MnCr5 and 20MnCr5, 18CrNiMo7-6 has considerably higher hardenability and core toughness: nickel improves toughness, while chromium and molybdenum carry hardenability into larger sections. It is therefore chosen for large modules, heavy shock loads and sections where MnCr grades no longer harden sufficiently in the core. EN ISO 683-3 specifies the grade by chemical composition, by hardenability (variants +H, +HH and +HL with Jominy bands) and by hardness in the delivery condition: soft annealed +A ≤ 229 HB, or treated to a ferrite-pearlite structure +FP 159–207 HB, which gives consistent machinability and predictable distortion. Tensile properties of the core after case hardening depend on section size and process, so they are not given here as a single table. Guideline values: carburizing at about 880–980 °C, core hardening from about 830–870 °C or case hardening from about 780–820 °C, tempering at 150–200 °C. The surface is typically targeted at 58–62 HRC; the case depth is specified on the drawing. There is no direct AISI/SAE equivalent; NiCrMo carburizing grades such as 4320 or 9310 are sometimes compared, but their Ni/Cr/Mo balance differs. Aktif Çelik quotes 18CrNiMo7-6 through its supply network as hot-rolled and forged round bar (+A or +FP); size, delivery condition, hardenability band, quantity and lead time are confirmed in the quotation, and deliveries can be made with an EN 10204 3.1 inspection certificate.

Related technical article: 18CrNiMo7-6

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
EN18CrNiMo7-6
W.-Nr. (DIN)1.6587
DIN 17210 (old)17CrNiMo6

Steel Equivalence Tables

Applications

  • Large, heavily loaded gears and pinions
  • Industrial and wind-turbine gearbox components
  • Gear shafts and ring gears
  • Transmissions for mining and construction machinery
  • Carburized shafts, splines and couplings
  • Heavy-duty carburized pins and bushes

Frequently Asked Questions

Is 18CrNiMo7-6 the same as 17CrNiMo6?+

They share the material number 1.6587: the old DIN 17210 name 17CrNiMo6 was replaced by 18CrNiMo7-6 in EN 10084. The new name follows EN 10027-1, where 7 and 6 are the Cr and Ni contents multiplied by 4 (about 1.75% Cr and 1.5% Ni). Old drawings that still cite 17CrNiMo6 should be checked against the current EN ISO 683-3 ranges.

Should I choose 18CrNiMo7-6 or 20MnCr5?+

18CrNiMo7-6 offers higher hardenability and core toughness and is preferred for large sections, large modules and shock-loaded gears. 20MnCr5 and 16MnCr5 are sufficient for small and medium gears and, without nickel and molybdenum, are more economical.

What do the +FP and +A delivery conditions mean?+

+FP means treated to a ferrite-pearlite structure within a defined hardness range (159–207 HB); it is chosen in gear manufacturing for consistent machinability and predictable heat-treatment distortion. +A is soft annealed (≤ 229 HB). If guaranteed hardenability is required, specify the +H, +HH or +HL variant on the order.

Is there an AISI equivalent of 18CrNiMo7-6?+

There is no direct one. NiCrMo carburizing steels such as AISI 4320 or 9310 are sometimes compared, but their nickel, chromium and molybdenum contents differ; the choice should be based on the required hardenability and core strength.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).