Steel Grade Datasheet

17NiCrMo6-4/ 1.6566Nickel-Chromium-Molybdenum Case Hardening Steel (EN ISO 683-3)

Standard
EN ISO 683-3
Delivery Conditions
+A, +TH, +FP
Density
7.85 g/cm³
W.-Nr.
1.6566

What is 17NiCrMo6-4 steel?

17NiCrMo6-4 (material no. 1.6566) is a nickel-chromium-molybdenum case hardening steel to EN ISO 683-3 (formerly EN 10084). It contains 0.14–0.20% carbon, 1.20–1.50% nickel, 0.80–1.10% chromium and 0.15–0.25% molybdenum, and in Italy it is known by its old UNI 7846 name 18NiCrMo5. After carburizing, quenching and low-temperature tempering it combines a hard, wear-resistant surface with a tough core. It is used for medium and heavily loaded gears, pinions and shafts. Delivery hardness is max. 229 HB in +A and 149–201 HB in +FP.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.14–0.20
Si≤ 0.40
Mn0.60–0.90
P≤ 0.025
S≤ 0.035
Cr0.80–1.10
Mo0.15–0.25
Ni1.20–1.50

Mechanical Properties

Hardness by Delivery Condition

Hardness limits given by the standard for these delivery conditions; certified values are stated on the inspection certificate (EN 10204 3.1).

Delivery conditionHardness
+A≤ 229 HB
+TH179–229 HB
+FP149–201 HB

Hardness: +A: ≤ 229 HB · +TH: 179–229 HB · +FP: 149–201 HB (EN ISO 683-3) · Carburized and hardened surface: typically 58–62 HRC, process-dependent

17NiCrMo6-4 / 1.6566 properties and use

Among case hardening steels, 17NiCrMo6-4 sits between MnCr grades such as 16MnCr5 / 20MnCr5 and the higher-alloyed 18CrNiMo7-6. Nickel raises core toughness and impact strength after case hardening, while chromium and molybdenum support hardenability. That is why it is chosen for impact-loaded gears and pinions where MnCr steels fall short. EN ISO 683-3 gives no tensile values for this grade in the delivery condition; core strength after case hardening depends on section and process, so this page shows the hardness table by delivery condition instead. Typical case hardening values (guide values from producer datasheets): carburizing at 880–980 °C, core hardening at 830–870 °C, case hardening at 780–820 °C, tempering at 150–200 °C. For machining, choose +A (soft annealed); if a defined hardness range is needed, order +TH (179–229 HB), or +FP (149–201 HB) for a ferrite-pearlite structure with a narrow hardness band. The variant with controlled sulphur, 17NiCrMoS6-4 (1.6569), improves machinability. Aktif Çelik supplies 17NiCrMo6-4 as hot-rolled and peeled round bars and as forged bars, from stock or through its production partners depending on size and quantity; whether a given size is in stock, the delivery condition, the minimum quantity and the lead time are stated in the quotation. Deliveries come with an EN 10204 3.1 inspection certificate; third-party inspection by bodies such as SGS, Bureau Veritas or TÜV can be arranged on request.

Related technical article: 17NiCrMo6-4

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
EN17NiCrMo6-4
W.-Nr. (DIN)1.6566
UNI 7846 (old, Italy)≈ 18NiCrMo5
EN (S variant)17NiCrMoS6-4 (1.6569)
BS 970 (UK)≈ 815M17 (EN353)

Steel Equivalence Tables

Applications

  • Medium and heavily loaded gears and pinions
  • Gearbox and differential parts
  • Gear shafts and splined shafts
  • Power-transmission parts for construction and agricultural machinery
  • Impact-loaded pins, bushings and rollers
  • General case-hardened machine parts

Frequently Asked Questions

Are 17NiCrMo6-4 and 18NiCrMo5 the same steel?+

18NiCrMo5 is the name in the old Italian standard UNI 7846; in EN ISO 683-3 this grade is covered by 17NiCrMo6-4 (1.6566), and in Italy both names are used interchangeably. The composition ranges are very close, but the two standards are not identical, so the table shows it with '≈'. The applicable standard should be named in the order.

What is the difference between 17NiCrMo6-4 and 18CrNiMo7-6 (17CrNiMo6)?+

Despite the similar names, they are different steels. 18CrNiMo7-6 (old DIN name 17CrNiMo6, 1.6587) has more chromium (1.50–1.80%), nickel (1.40–1.70%) and molybdenum (0.25–0.35%); its deeper hardenability makes it the choice for large-module, large-section gears. 17NiCrMo6-4 (1.6566) is lower alloyed and more economical for medium sections. Stating the material number in an enquiry avoids confusion.

Why choose 17NiCrMo6-4 instead of 16MnCr5?+

16MnCr5 contains no nickel. The 1.20–1.50% nickel in 17NiCrMo6-4 raises core toughness and impact strength after case hardening, and molybdenum supports hardenability. For impact-loaded gears, larger sections or parts that need a higher safety margin, this difference is decisive; for small parts with light to medium loads, 16MnCr5 is usually sufficient and more economical.

What do the +A, +TH and +FP delivery conditions mean?+

+A is soft annealed (max. 229 HB) and eases machining. +TH is treated to a defined hardness range (179–229 HB). +FP is treated to a ferrite-pearlite structure within 149–201 HB; it is preferred for series machining and for dimensional stability during case hardening. The required condition should be stated in the order.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).