Steel Grade Datasheet

50CrMo4/ 1.7228 / ≈ 4150Chromium-Molybdenum Q&T Steel (EN 10083-3)

Standard
EN 10083-3
Delivery Conditions
+A, +QT
Density
7.85 g/cm³
W.-Nr.
1.7228

What is 50CrMo4 steel?

50CrMo4 (material no. 1.7228) is a chromium-molybdenum alloy steel for quenching and tempering to EN 10083-3. It contains 0.46–0.54% carbon, 0.90–1.20% chromium and 0.15–0.30% molybdenum, which makes it the higher-carbon sibling of 42CrMo4. Quenched and tempered (+QT), it reaches a minimum yield strength of 900 MPa and a tensile strength of 1100–1300 MPa up to 16 mm; for 100–160 mm sections the values are 650 MPa and 850–1000 MPa. It is used for heavily loaded shafts, gears and forgings that need high strength, good hardenability and a higher surface hardness than 42CrMo4.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.46–0.54
Si≤ 0.40
Mn0.50–0.80
P≤ 0.025
S≤ 0.035
Cr0.90–1.20
Mo0.15–0.30

Mechanical Properties (+QT)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 169001100–13009
16 < d ≤ 407801000–120010
40 < d ≤ 100700900–110012
100 < d ≤ 160650850–100013
160 < d ≤ 250550800–95013

Hardness by Delivery Condition

Hardness limits given by the standard for these delivery conditions; certified values are stated on the inspection certificate (EN 10204 3.1).

Delivery conditionHardness
+A≤ 248 HB

Hardness: +A (soft annealed): max. 248 HB (EN 10083-3) · +QT: Rm 800–1300 MPa ≈ 235–385 HB (approximate conversion per EN ISO 18265; for +QT the standard specifies strength, not hardness).

50CrMo4 / 1.7228 properties and use

50CrMo4 shares the Cr-Mo alloy design of 42CrMo4; the difference is about 0.08% more carbon. Higher carbon gives more strength in the same section and a higher surface hardness after induction or flame hardening, at the cost of some toughness and weldability. Molybdenum gives resistance to temper embrittlement and supports hardenability in thick sections. The +QT values in EN 10083-3 depend on diameter: minimum yield strength is 900 MPa up to 16 mm, 700 MPa at 40–100 mm and 550 MPa at 160–250 mm. Typical heat treatment (guide values from producer datasheets): hardening at 820–860 °C in oil, tempering at 540–680 °C; soft annealing at 680–720 °C, normalizing at 850–880 °C. For machining, order the +A condition (soft annealed, max. 248 HB) and quench and temper the part after machining, or buy the bar directly in the +QT condition. Welding is not recommended; where it cannot be avoided, preheating and post-weld stress relieving are required. Aktif Çelik supplies 50CrMo4 as hot-rolled and peeled round bars and as forged bars, from stock or through its production partners depending on size and quantity; whether a given size is in stock, the delivery condition, the minimum quantity and the lead time are stated in the quotation. Deliveries come with an EN 10204 3.1 inspection certificate; third-party inspection by bodies such as SGS, Bureau Veritas or TÜV can be arranged on request.

Related technical article: 50CrMo4

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
EN50CrMo4
W.-Nr. (DIN)1.7228
AISI/SAE≈ 4150
BS 970 (UK)≈ 708A47

Steel Equivalence Tables

Applications

  • Heavily loaded shafts and axles
  • Induction-hardened gears, pinions and racks
  • Rings, bushings and tyres
  • Steering and control parts for vehicles and construction machinery
  • Large-section forged machine parts
  • High-strength parts for hydraulic and mining equipment

Frequently Asked Questions

What is the difference between 50CrMo4 and 42CrMo4?+

Both grades have the same chromium-molybdenum design; carbon is 0.46–0.54% in 50CrMo4 and 0.38–0.45% in 42CrMo4. Under EN 10083-3 both have a minimum yield strength of 900 MPa up to 16 mm; at 40–100 mm, 50CrMo4 gives 700 MPa and 42CrMo4 650 MPa. 50CrMo4 reaches a higher surface hardness and wear resistance after surface hardening; 42CrMo4 is tougher and easier to weld, which is why it is more common in general applications.

What is the AISI equivalent of 50CrMo4?+

The nearest match is AISI/SAE 4150. Carbon, chromium and molybdenum ranges are close, but manganese is 0.75–1.00% in 4150 against 0.50–0.80% in 50CrMo4, and the mechanical properties are defined by different standards. The nearest British BS 970 grade is 708A47. That is why the table shows these equivalents with '≈'; any substitution should be approved after comparing the order standard.

Can 50CrMo4 be induction hardened?+

Yes. Quenched and tempered (+QT) 50CrMo4 is suitable for induction or flame hardening; thanks to its higher carbon it reaches a higher surface hardness than 42CrMo4, while the core keeps its Q&T strength. The achievable hardness and case depth depend on section, prior heat treatment and process parameters, so target values should be stated in the order.

Can 50CrMo4 be welded?+

It is not a grade intended for welding. Its carbon and alloy content form a hard, crack-prone structure in the heat-affected zone. If welding is unavoidable, suitable preheating, low-hydrogen filler metal and post-weld stress relieving or re-hardening and tempering are needed; the procedure should be set by a welding engineer.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).