Steel Grade Datasheet

S275JR/ 1.0044Non-Alloy Structural Steel (EN 10025-2)

Standard
EN 10025-2
Delivery Conditions
+AR, +N
Density
7.85 g/cm³
W.-Nr.
1.0044

What is S275JR steel?

S275JR (material no. 1.0044, old DIN name St 44-2) is a non-alloy structural steel to EN 10025-2. '275' stands for a minimum yield strength of 275 MPa up to 16 mm thickness; 'JR' for a minimum impact energy of 27 J at +20 °C. Tensile strength is 410–560 MPa for 3–100 mm. With carbon of max. 0.21–0.22% and a carbon equivalent (CEV) of max. 0.40 up to 40 mm it welds well, and it is used for welded and bolted steel structures that need more strength than S235JR.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C≤ 0.21 (d ≤ 40) · ≤ 0.22 (d > 40)
Si—
Mn≤ 1.50
P≤ 0.035
S≤ 0.035
N≤ 0.012
Cu≤ 0.55
CEV≤ 0.40 (d ≤ 40) · ≤ 0.42 (40 < d ≤ 150)

Mechanical Properties (+AR / +N)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 16275410–56023
16 < d ≤ 40265410–56023
40 < d ≤ 63255410–56022
63 < d ≤ 80245410–56021
80 < d ≤ 100235410–56021
100 < d ≤ 150225400–54019

Hardness: EN 10025-2 does not specify hardness. A tensile strength of 410–560 MPa corresponds to roughly 120–165 HB (approximate conversion per EN ISO 18265, not a standard value).

S275JR / 1.0044 properties and use

S275JR sits in the middle of the common EN 10025-2 strength classes, between S235 and S355. Yield strength falls as thickness increases (275 MPa up to 16 mm, 225 MPa at 100–150 mm), so design must use the value for the actual thickness. The JR quality defines the impact test at +20 °C with 27 J; for structures working at lower temperatures, S275J0 (0 °C) or S275J2 (−20 °C) is chosen. Weldability is secured in the standard by a carbon-equivalent limit: CEV max. 0.40 up to 40 mm and max. 0.42 for 40–150 mm. At this level thin and medium sections are usually welded without preheat; for thick sections and rigid joints the need for preheat is determined to EN 1011-2. Delivery conditions are +AR (as rolled) or +N (normalized or normalized rolled). Name conversion: S275JR replaces St 44-2 of the old DIN 17100 and grade 43B of the British BS 4360. Aktif Çelik supplies S275JR as hot-rolled round, square and flat bars and sections, from stock or through its production partners depending on size and quantity; whether a given size is in stock, the minimum quantity and the lead time are stated in the quotation. Deliveries come with an EN 10204 3.1 inspection certificate; third-party inspection by bodies such as SGS, Bureau Veritas or TÜV can be arranged on request.

Related technical article: S275JR

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
ENS275JR
W.-Nr. (DIN)1.0044
DIN 17100 (old)St 44-2
BS 4360 (old)43B
AFNOR (old)E28-2
UNI (old)Fe 430 B
ASTM≈ A36
JIS≈ SS400
GB (China)≈ Q275B

Steel Equivalence Tables

Applications

  • Steel structures and load-bearing members
  • Welded frames, platforms and stairs
  • Machine chassis, bases and housings
  • Connection plates, flats and brackets
  • Agricultural, construction and handling equipment
  • General fabrication with bolted joints

Frequently Asked Questions

What is the difference between S275JR, S235JR and S355J2?+

The difference is yield strength and impact class. Minimum yield strength up to 16 mm is 235 MPa for S235JR, 275 MPa for S275JR and 355 MPa for S355J2. S235JR and S275JR are impact tested at +20 °C (JR), S355J2 at −20 °C (J2). S275JR carries the same load as S235JR with lighter sections; where higher strength or low-temperature toughness is needed, S355J2 is chosen.

What is the old name of S275JR?+

The old DIN 17100 name is St 44-2; the material number 1.0044 is unchanged. It appears as 43B in British BS 4360, as E28-2 in French NF A 35-501 and as Fe 430 B in the old Italian and European designation. 'St 44' refers to the approximate tensile strength (kp/mm²), 'S275' to the yield strength (MPa).

Is there an ASTM or JIS equivalent of S275JR?+

There is no exact equivalent. ASTM A36 and JIS SS400 are often compared, but their yield, tensile and impact requirements differ; A36, for example, has a minimum yield strength of 250 MPa, below the 275 MPa of S275JR up to 16 mm. Any substitution should be approved by an engineer after comparing the project standard and the required values.

Can S275JR be welded, and is preheat needed?+

Yes, it welds well. With CEV max. 0.40 up to 40 mm, thin and medium thicknesses are usually welded without preheat. For thick sections, low ambient temperature or high restraint, the need for preheat is determined to EN 1011-2; the carbon equivalent calculator on our site can be used for a first assessment.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.