Steel Grade Datasheet

36CrNiMo4/ 1.6511 / ≈ 9840Nickel-Chromium-Molybdenum Q&T Steel (EN 10083-3)

Standard
EN 10083-3
Delivery Conditions
+A, +QT
Density
7.85 g/cm³
W.-Nr.
1.6511

What is 36CrNiMo4 steel?

36CrNiMo4 (material no. 1.6511) is a nickel-chromium-molybdenum alloy steel for quenching and tempering to EN 10083-3. It contains 0.32–0.40% carbon, 0.90–1.20% chromium, 0.90–1.20% nickel and 0.15–0.30% molybdenum. Quenched and tempered (+QT), it gives a minimum yield strength of 900 MPa and a tensile strength of 1100–1300 MPa up to 16 mm; for 100–160 mm sections the values are 600 MPa and 800–950 MPa. Its nickel gives higher core toughness than Cr-Mo steels, and it is used for medium and large shafts, gears and forgings.

Chemical Composition

Cast analysis, % by weight (per the applicable EN standard)

ElementRange (%)
C0.32–0.40
Si≤ 0.40
Mn0.50–0.80
P≤ 0.025
S≤ 0.035
Cr0.90–1.20
Mo0.15–0.30
Ni0.90–1.20

Mechanical Properties (+QT)

Values depend on ruling section / thickness (d).

Section (mm)Yield Re min (MPa)Tensile Rm (MPa)Elongation A min (%)
d ≤ 169001100–130010
16 < d ≤ 408001000–120011
40 < d ≤ 100700900–110012
100 < d ≤ 160600800–95013

Hardness by Delivery Condition

Hardness limits given by the standard for these delivery conditions; certified values are stated on the inspection certificate (EN 10204 3.1).

Delivery conditionHardness
+A≤ 248 HB

Hardness: +A (soft annealed): max. 248 HB (EN 10083-3) · +QT: Rm 800–1300 MPa ≈ 235–385 HB (approximate conversion per EN ISO 18265; for +QT the standard specifies strength, not hardness).

36CrNiMo4 / 1.6511 properties and use

Among the EN 10083-3 Q&T steels, 36CrNiMo4 sits between Cr-Mo grades such as 42CrMo4 and 34CrNiMo6: about 1% nickel is added to a Cr-Mo design, while nickel and chromium stay below those of 34CrNiMo6. Nickel raises core toughness and impact strength after quenching and tempering; chromium and molybdenum support hardenability, and molybdenum also reduces temper embrittlement. The +QT values depend on diameter: minimum yield strength is 900 MPa up to 16 mm, 800 MPa at 16–40 mm, 700 MPa at 40–100 mm and 600 MPa at 100–160 mm. Typical heat treatment (guide values): hardening at about 820–860 °C in oil or water, tempering at 540–680 °C. For machining, the steel is bought in the +A condition (soft annealed, max. 248 HB) and quenched and tempered after machining, or supplied directly as +QT. In Poland it is also known by its old PN name 36HNM. It is not a grade for welding; where welding is unavoidable, preheating and post-weld heat treatment are needed. Aktif Çelik supplies 36CrNiMo4 as forged bars and forgings and as hot-rolled and peeled round bars, from stock or through its production partners depending on size and quantity; whether a given size is in stock, the delivery condition, the minimum quantity and the lead time are stated in the quotation. Deliveries come with an EN 10204 3.1 inspection certificate; third-party inspection by bodies such as SGS, Bureau Veritas or TÜV can be arranged on request.

Related technical article: 36CrNiMo4

International Equivalents

Values marked ≈ are nearest matches, not exact equivalents. Always confirm against the governing standard.

SystemGrade
EN36CrNiMo4
W.-Nr. (DIN)1.6511
PN (Poland, old)≈ 36HNM
AISI/SAE≈ 9840
BS 970 (UK)≈ 816M40 (EN110)

Steel Equivalence Tables

Applications

  • Medium and large-section shafts and axles
  • Heavily loaded gears and gear shafts
  • Connecting rods and dynamically loaded forgings
  • High-strength bolts, studs and fasteners
  • Hydraulic and construction machinery parts
  • Machine and vehicle parts subject to impact loads

Frequently Asked Questions

What is the difference between 36CrNiMo4 and 34CrNiMo6?+

Both are Ni-Cr-Mo Q&T steels; nickel and chromium are 1.30–1.70% in 34CrNiMo6 and 0.90–1.20% in 36CrNiMo4. The higher alloy content gives 34CrNiMo6 deeper hardenability: under EN 10083-3 the minimum yield strength up to 16 mm is 1000 MPa for 34CrNiMo6 and 900 MPa for 36CrNiMo4, and at 100–160 mm it is 700 MPa against 600 MPa. Where medium sections do not need the full capacity of 34CrNiMo6, 36CrNiMo4 is the more economical choice.

What is the AISI equivalent of 36CrNiMo4 — is it 4340?+

There is no exact AISI equivalent. The nearest grade is the old SAE 9840, which is no longer common. AISI 4340, with 1.65–2.00% nickel, is closer to 34CrNiMo6 and is not an equivalent of 36CrNiMo4. The nearest British BS 970 grade is 816M40 (EN110) and the Polish one is 36HNM; all are shown with '≈' in the table.

Up to which section size can 36CrNiMo4 be quenched and tempered?+

EN 10083-3 gives the +QT values by diameter, and strength falls as the section grows: minimum yield strength is 900 MPa up to 16 mm and 600 MPa at 100–160 mm. For larger sections that need high core strength, the higher-alloyed 34CrNiMo6 or 30CrNiMo8 should be considered. Required values and the test-piece location should be stated in the order.

Are 36HNM and 36CrNiMo4 the same steel?+

36HNM is the name in the old Polish standard PN-89/H-84030/04, and its chemistry is very close to 36CrNiMo4; today Poland uses the EN 10083-3 name 36CrNiMo4. Because the ranges are not identical (for example the phosphorus and molybdenum limits), the table shows it with '≈'; the applicable standard should be named in the order.

Looking for this steel grade?

Request a quote with your sizes, tolerances and delivery condition — we respond within 24 hours.

Request a Quote

Related Tools

Values on this page are reference data compiled from the applicable EN standard; certified material properties are defined by the mill test certificate (EN 10204 3.1).